True Strain Calculator

Convert engineering strain to true (logarithmic) strain and true stress from strain, lengths or area, and see how far the two measures drift apart.

📏 True Strain Calculator
Engineering strain (e)
%
0100
Engineering stress (optional)
MPa
01000
Original length (L0)
mm
Current length (L)
mm
25100
Engineering stress (optional)
MPa
Original diameter (d0)
mm
Current diameter (d)
mm
120
Axial force (optional)
kN
True strain (ε)
01.5
True stress (optional)
MPa
01500
True strain
—
True strain (%)
—
Engineering strain
—
Difference (e minus true)
—
Engineering overstates by
—
True stress
—
Length ratio L/L0
—
Area ratio A/A0
—

True strain ln(L/L0)
—
True strain (%)
—
Engineering strain
—
Length ratio L/L0
—
Difference (e minus true)
—
True stress
—
Change in length
—
Area ratio A/A0
—

True strain ln(A0/A)
—
True strain (%)
—
Engineering strain
—
Reduction in area
—
True stress F/A
—
Engineering stress F/A0
—
Original area
—
Current area
—

Engineering strain
—
True strain
—
True strain (%)
—
Difference (e minus true)
—
Length ratio L/L0
—
Engineering stress
—
True stress
—

📏 What is True Strain?

True strain, also called logarithmic strain or natural strain, measures deformation by adding up many tiny strain increments, each one taken relative to the length the sample has at that moment. If a bar grows from L0 to L, the true strain is the natural logarithm of the length ratio, ln(L/L0). Engineering strain, in contrast, divides the whole change in length by the original length only, (L - L0)/L0. The two agree for small deformations and drift apart as the stretch gets larger.

True strain matters wherever materials are deformed a lot: metal forming, wire drawing, rolling, extrusion, forging and the plastic part of a tensile test. Materials scientists fit flow curves such as the Hollomon relation to true stress and true strain, because those measures describe the material's response at the instantaneous cross section instead of an out-of-date reference. Another practical reason to prefer it is additivity: if you stretch a bar by 10 percent and then another 10 percent, the true strains add (2 ln 1.1 = 0.1906), while the engineering strains do not combine by simple addition. A compression and an extension of the same amount also have equal and opposite true strains, which engineering strain cannot offer.

A few distinctions help avoid mistakes. True strain is not the same as the plastic strain or the strain at fracture, although it can be used to express both. True stress is the force divided by the current area, not the original area, and for uniform constant-volume deformation it equals engineering stress times (1 + e). Both conversions assume the deformation is uniform along the gauge length, so they stop being valid once a tensile bar begins to neck. In a necked bar the area at the neck is the correct quantity, which is why the area-based form ln(A0/A) is used for the strain at fracture.

This calculator converts in four ways. Start from engineering strain, from measured lengths, from the diameters of a round bar, or run the conversion backwards from a true strain. Each mode returns the true strain, the engineering strain, the stress conversion if you give a stress, and a chart of the relationship. The first mode also prints a conversion table so you can see exactly how much the two measures differ at 1, 5, 10 or 50 percent.

📐 Formula

εt  =  ln(1 + e)  =  ln(L / L0)  =  ln(A0 / A)
εt = true (logarithmic) strain, dimensionless
e = engineering strain = (L − L0) / L0, entered here in percent
L0, L = original and current gauge length
A0, A = original and current cross-sectional area; A0/A = L/L0 only when the volume is constant
True stress: σt = σe (1 + e) = F / A
Inverse: e = exp(εt) − 1 and σe = σt / (1 + e)
Example: e = 20 % gives εt = ln 1.2 = 0.18232, and 400 MPa engineering stress becomes 480 MPa true stress

📖 How to Use This Calculator

Steps

1
Choose how you know the deformation. Pick Engineering to true if you have the engineering strain, From lengths if you measured L0 and L, From area for the diameters of a round bar, or True to engineering to convert backwards.
2
Enter the values. Type the strain in percent (or true strain as a plain number), lengths or diameters in mm, and optionally a stress in MPa or a force in kN if you also want the true stress.
3
Read the result and chart. The big number is the main conversion. Below it are the difference between the two measures, the stress conversion, a conversion table in the first mode, and a chart with your point marked.

💡 Example Calculations

Example 1 — 20 Percent Engineering Strain

e = 20 %, engineering stress 400 MPa

1
1 + e = 1.2, so the true strain is ln(1.2) = 0.18232 (18.23 %)
2
True stress = 400 × 1.2 = 480.0 MPa
3
The engineering value is 1.77 percentage points higher, so it overstates the true strain by 9.7 %.
True strain = 0.18232, true stress = 480.0 MPa
Try this example →

Example 2 — A Small Elastic Strain

e = 2 %, engineering stress 250 MPa

1
ln(1.02) = 0.019803, which is 1.980 % true strain
2
The difference from 2.000 % is only 0.0197 percentage points, a 1.0 % overstatement
3
True stress = 250 × 1.02 = 255.0 MPa. At small strain the two measures are practically identical.
True strain = 0.019803, true stress = 255.0 MPa
Try this example →

Example 3 — Stretched Strip from Measured Lengths

L0 = 50 mm stretched to L = 65 mm, engineering stress 350 MPa

1
L/L0 = 65 / 50 = 1.3, so the engineering strain is 30.00 %
2
True strain = ln(1.3) = 0.26236 (26.24 %), a difference of 3.76 percentage points
3
True stress = 350 × 1.3 = 455.0 MPa, and the area has shrunk to 0.7692 of its original value
True strain = 0.26236, true stress = 455.0 MPa
Try this example →

Example 4 — Necked Tensile Bar from Diameters

d0 = 12.5 mm reduced to d = 8 mm at the neck, force 30 kN

1
A0 = π × 12.5² / 4 = 122.72 mm² and A = π × 8² / 4 = 50.27 mm²
2
True strain = ln(122.72 / 50.27) = 0.89257, which equals 2 ln(12.5 / 8). The reduction in area is 59.04 %.
3
True stress = 30000 / 50.27 = 596.8 MPa, against 244.5 MPa engineering stress (30000 / 122.72)
True strain = 0.89257, true stress = 596.8 MPa
Try this example →

Example 5 — Back from True to Engineering

True strain 0.5, true stress 700 MPa

1
e = exp(0.5) − 1 = 1.6487 − 1 = 64.872 %
2
The two measures differ by 14.9 percentage points at this deformation
3
Engineering stress = 700 / 1.6487 = 424.6 MPa
Engineering strain = 64.872 %, engineering stress = 424.6 MPa
Try this example →

❓ Frequently Asked Questions

What is the formula for true strain?+
True strain is epsilon = ln(1 + e), where e is the engineering strain written as a ratio. Equivalently epsilon = ln(L/L0). For 20 percent engineering strain the true strain is ln(1.2) = 0.1823, a little less than the engineering value of 0.20.
How do you convert engineering strain to true strain?+
Add 1 to the engineering strain ratio and take the natural logarithm. For e = 0.35 the true strain is ln(1.35) = 0.3001. To go back, use e = exp(epsilon) minus 1. The True to engineering mode of this calculator does that direction.
How do you calculate true stress from engineering stress?+
With constant volume and uniform deformation, true stress equals engineering stress times (1 + e). An engineering stress of 400 MPa at 20 percent strain corresponds to a true stress of 480 MPa. The result is just force divided by the current area instead of the original area.
Why is true strain smaller than engineering strain in tension?+
True strain adds small increments dL/L measured against the current length, which keeps growing, while engineering strain divides the whole change by the original length. Since ln(1 + e) is less than e for any positive e, the true strain is always the smaller of the two in tension.
What is the area-based formula for true strain?+
For constant volume A L is constant, so L/L0 = A0/A and epsilon = ln(A0/A). For a round bar this equals 2 ln(d0/d). It is the preferred form after necking because the minimum diameter can still be measured, whereas the gauge length no longer represents the local strain.
When do engineering and true strain differ significantly?+
At 1 percent strain they differ by about 0.5 percent of the value, at 10 percent by about 5 percent, and at 50 percent by about 23 percent. Beyond roughly 10 percent strain the difference matters for forming analysis. The conversion table in the first mode lists several values.
Does true strain work after necking?+
The formulas assume uniform deformation along the gauge length. After necking the strain is concentrated in the neck, so a gauge-length value no longer represents the local strain. Use the area-based form with the measured neck area instead, and treat the stress conversion sigma(1+e) as invalid past that point.
Can true strain be negative?+
Yes. In compression the length ratio is below 1, so ln(L/L0) is negative. A bar compressed to half its length has a true strain of ln(0.5) = -0.693, whereas its engineering strain is -0.5. Enter a negative engineering strain in the first mode to see this.
Why do true strains add up but engineering strains do not?+
Because ln(L2/L0) = ln(L1/L0) + ln(L2/L1). Two successive stretches multiply the length ratios, and the logarithm turns that product into a sum. Two successive 10 percent stretches give a true strain of 0.1906 but an overall engineering strain of 21 percent.
Why is true stress higher than engineering stress?+
As a bar stretches its cross-sectional area shrinks, so the same force acts on a smaller area. Engineering stress uses the original area, true stress uses the current one, so in tension true stress is larger by the factor (1 + e) when volume is constant.
At what strain does necking start?+
Necking begins at the ultimate tensile strength, where the work hardening rate equals the true stress (the Considere criterion). For a material following a power law sigma = K epsilon^n, the true strain at necking equals the hardening exponent n. The value depends on the material and is not computed here.
Does the calculator assume constant volume?+
The stress conversion and the area form do, since both rely on A L being constant (a Poisson ratio of 0.5). The strain conversions ln(1 + e) and ln(L/L0) are exact definitions and do not depend on that assumption. Elastic deformation of metals changes volume slightly, which is negligible at large plastic strains.

What is the formula for true strain?

True strain is epsilon = ln(1 + e), where e is the engineering strain (change in length over original length) written as a ratio. Equivalently epsilon = ln(L/L0). For 20 percent engineering strain the true strain is ln(1.2) = 0.1823.

How do you convert engineering strain to true strain?

Add 1 to the engineering strain ratio and take the natural logarithm. For e = 0.35 the true strain is ln(1.35) = 0.3001. To go back, use e = exp(epsilon) - 1. The calculator does both directions.

How do you calculate true stress from engineering stress?

With constant volume and uniform deformation, true stress equals engineering stress times (1 + e). An engineering stress of 400 MPa at 20 percent strain corresponds to 480 MPa true stress.

Why is true strain smaller than engineering strain in tension?

True strain adds up small increments dL/L measured on the current length, which keeps growing, while engineering strain divides the whole change by the original length. Since ln(1 + e) is less than e for e above zero, true strain is smaller.

What is the area-based formula for true strain?

For constant volume, A L is constant so L/L0 = A0/A and epsilon = ln(A0/A). For a round bar this equals 2 ln(d0/d). It is the preferred form after necking because the minimum diameter can still be measured.

When do engineering and true strain differ significantly?

At 1 percent strain they differ by 0.5 percent of the value, at 10 percent by about 5 percent, and at 50 percent by about 23 percent. Beyond roughly 10 percent strain the difference is important for forming analysis.

Does true strain work after necking?

The formulas assume uniform deformation. After necking the strain is concentrated in the neck, so a gauge-length based value no longer represents the local strain. Use the area-based form with the measured neck area instead.

Can true strain be negative?

Yes. In compression the length ratio is below 1, so ln(L/L0) is negative. A bar compressed to half its length has a true strain of ln(0.5) = -0.693, whereas its engineering strain is -0.5.