Mooney-Rivlin Model Calculator

Evaluate the two-parameter Mooney-Rivlin rubber model for stress and shear modulus, or fit C10 and C01 from a Mooney plot.

📈 Mooney-Rivlin Model Calculator
Constant C10
MPa
Constant C01
MPa
Stretch ratio (λ)
Point 1 stretch (λ1)
Point 1 engineering stress
MPa
Point 2 stretch (λ2)
Point 2 engineering stress
MPa
Engineering stress (uniaxial)
—
True (Cauchy) stress
—
Shear modulus μ = 2(C10 + C01)
—
Young modulus E ≈ 3μ
—
Reduced stress s*
—
Neo-Hookean (same μ)
—
Difference from neo-Hookean
—
Equibiaxial stress, same λ
—

Constant C10 (intercept)
—
Constant C01 (slope)
—
Shear modulus μ
—
Young modulus E ≈ 3μ
—
C01 / C10
—
C10 if C01 = 0
—

📈 What is the Mooney-Rivlin Model?

The Mooney-Rivlin model is a two-parameter constitutive law for rubber-like materials. Melvin Mooney proposed it in 1940 for the stress-stretch response of vulcanized rubber, and Ronald Rivlin later wrote it in terms of the strain invariants. For an incompressible solid its strain energy density is W = C10 (I1 − 3) + C01 (I2 − 3), where I1 and I2 are the first two invariants of the deformation and C10 and C01 are material constants with units of stress. When C01 is zero the second term disappears and the model collapses to the neo-Hookean solid, which follows directly from the statistical theory of Gaussian network chains.

The extra constant gives the model the flexibility to follow real data more closely. Rubber in tension often shows a modulus that is high at small stretch, falls through a minimum and then rises again. Plotted as a Mooney plot, with the reduced stress s* = s / (2(λ − λ−2)) against 1/λ, the data lie close to a straight line whose intercept is C10 and whose slope is C01. A flat line is neo-Hookean behavior. A sloped line, usually with positive C01, means the neo-Hookean model underpredicts the stiffness at small stretch and overpredicts the stress at larger stretch.

The initial shear modulus is μ = 2 (C10 + C01), so the small-strain Young modulus of an incompressible rubber is about 3μ. The individual constants are not separately measurable physical quantities; they are fitting parameters that depend on the stretch range, and two different pairs can yield the same modulus. For that reason you should quote the range of stretch over which a fit was made and prefer several data points over two. The two-point fit here is a quick way to extract the constants and to see the Mooney plot, not a replacement for a proper nonlinear least-squares fit to a full test.

This calculator offers two modes. The first evaluates the uniaxial stress, the shear modulus, the comparison with a neo-Hookean solid of the same modulus and the equibiaxial stress at the same stretch. The second fits C10 and C01 from two measured points. For the one-parameter case and the link to crosslink density see the rubber elasticity (neo-Hookean) stress calculator, and for the modulus relations see the shear modulus calculator.

📐 Formula

s  =  2 (λ − λ−2) (C10 + C01 / λ)    μ = 2 (C10 + C01)
s = uniaxial engineering (nominal) stress; the true stress is σ = s λ
λ = stretch ratio, current length over original length
C10, C01 = Mooney-Rivlin constants (MPa); μ = initial shear modulus, E ≈ 3μ
Neo-Hookean limit: C01 = 0, giving s = μ (λ − λ−2) with μ = 2 C10
Equibiaxial: s = 2 (λ − λ−5)(C10 + C01 λ2)
Example: C10 = 0.25, C01 = 0.10 MPa, λ = 2 give s = 1.050 MPa
s*  =  s ÷ (2 (λ − λ−2))  =  C10 + C01 (1/λ)
s* = reduced (Mooney) stress; plotted against 1/λ it is a straight line
Slope: C01 = (s*1 − s*2) / (1/λ1 − 1/λ2)
Intercept: C10 = s*1 − C01 / λ1
Example: (1.5, 0.6685 MPa) and (3.0, 1.637 MPa) give C10 = 0.2500 and C01 = 0.1000 MPa

📖 How to Use This Calculator

Two modes

1
Choose a mode - Pick Stress from constants to evaluate the model for given C10, C01 and stretch, or Fit from data to find C10 and C01 from two points.
2
Enter the values - Type C10 and C01 in MPa with the stretch ratio, or two pairs of stretch ratio and engineering stress in MPa. C01 may be zero or negative.
3
Read the results - Read the stress, the shear modulus and the neo-Hookean comparison, or the fitted constants and their ratio.
4
Check the chart - The stress chart compares Mooney-Rivlin with a neo-Hookean solid of the same modulus. The Mooney plot shows the fitted line and its flat neo-Hookean counterpart.

💡 Example Calculations

Example 1 - Stress at twice the length

C10 = 0.25 MPa, C01 = 0.10 MPa (illustrative constants), λ = 2

1
λ − λ−2 = 2 − 0.25 = 1.75 and C10 + C01/λ = 0.25 + 0.05 = 0.30.
2
s = 2 × 1.75 × 0.30 = 1.050 MPa and the true stress is 2.100 MPa. The shear modulus is μ = 2 × 0.35 = 0.7000 MPa.
3
A neo-Hookean solid with the same μ gives 0.7 × 1.75 = 1.225 MPa, so Mooney-Rivlin is 14.29 percent lower. The equibiaxial stress at the same λ is 2.559 MPa.
s = 1.050 MPa, μ = 0.7000 MPa, vs neo-Hookean -14.29 %
Try this example →

Example 2 - The neo-Hookean limit

C10 = 0.30 MPa, C01 = 0, λ = 1.5

1
λ − λ−2 = 1.5 − 0.4444 = 1.0556.
2
s = 2 × 1.0556 × 0.30 = 0.6333 MPa, with μ = 0.6000 MPa and true stress 0.9500 MPa.
3
The neo-Hookean value with the same μ is identical, 0.6333 MPa, so the difference is 0.00 percent.
s = 0.6333 MPa, difference = 0.00 %
Try this example →

Example 3 - Fitting C10 and C01 from two points

(λ, s) = (1.5, 0.6685 MPa) and (3.0, 1.637 MPa)

1
Reduced stresses: s*1 = 0.6685 / (2 × 1.0556) = 0.3167 MPa and s*2 = 1.637 / (2 × 2.8889) = 0.2833 MPa.
2
Slope C01 = (0.3167 − 0.2833) / (0.6667 − 0.3333) = 0.1000 MPa.
3
Intercept C10 = 0.3167 − 0.1000 × 0.6667 = 0.2500 MPa, so μ = 0.7000 MPa, E ≈ 2.100 MPa and C01/C10 = 0.4000.
C10 = 0.2500 MPa, C01 = 0.1000 MPa
Try this example →

Example 4 - A fit with a negative C01

(λ, s) = (1.5, 0.6685 MPa) and (2.5, 1.5444 MPa)

1
Reduced stresses: s*1 = 0.3167 MPa and s*2 = 1.5444 / (2 × 2.34) = 0.3300 MPa.
2
Slope C01 = (0.3167 − 0.3300) / (0.6667 − 0.4000) = -0.0500 MPa, so the Mooney plot tilts downward.
3
C10 = 0.3167 + 0.0500 × 0.6667 = 0.3500 MPa, μ = 0.6000 MPa, and C01/C10 = -0.1429. If C01 were forced to zero the average C10 would be 0.3233 MPa.
C10 = 0.3500 MPa, C01 = -0.0500 MPa
Try this example →

❓ Frequently Asked Questions

What is the Mooney-Rivlin model?+
The Mooney-Rivlin model is a two-parameter hyperelastic law for rubber with strain energy W = C10 (I1 - 3) + C01 (I2 - 3). It reduces to the neo-Hookean model when C01 = 0 and often fits uniaxial rubber data over a wider stretch range.
What is the uniaxial stress formula for a Mooney-Rivlin solid?+
The engineering stress is s = 2 (lambda - lambda^-2)(C10 + C01 / lambda). With C10 = 0.25 MPa, C01 = 0.10 MPa and lambda = 2, s = 2 x 1.75 x 0.30 = 1.050 MPa, and the true stress is s x lambda = 2.100 MPa.
How do you find the shear modulus from C10 and C01?+
The initial shear modulus is mu = 2 (C10 + C01). For C10 = 0.25 MPa and C01 = 0.10 MPa, mu = 0.70 MPa. The small-strain Young modulus of an incompressible rubber is about 3 mu, which is 2.1 MPa.
What is a Mooney plot?+
A Mooney plot graphs the reduced stress s* = s / (2 (lambda - lambda^-2)) against 1/lambda. For a Mooney-Rivlin solid this is a straight line with intercept C10 and slope C01. A horizontal line means neo-Hookean behavior.
How do you fit C10 and C01 from two data points?+
Compute the reduced stress at each stretch, then C01 = (s1* - s2*) / (1/lambda1 - 1/lambda2) and C10 = s1* - C01 / lambda1. For (1.5, 0.6685) and (3.0, 1.637) MPa this gives C10 = 0.2500 and C01 = 0.1000 MPa.
What is the neo-Hookean limit?+
Setting C01 = 0 gives the neo-Hookean model with mu = 2 C10, in which the Mooney plot is flat. The stress becomes s = 2 C10 (lambda - lambda^-2), so one constant describes the response.
What is the equibiaxial stress in the Mooney-Rivlin model?+
The engineering stress under equibiaxial stretch is s = 2 (lambda - lambda^-5)(C10 + C01 lambda^2). With C10 = 0.25, C01 = 0.10 MPa and lambda = 2 this is 2.559 MPa, noticeably higher than the uniaxial value because the C01 term grows with lambda squared.
Why is C01 sometimes negative?+
Fits to wide stretch ranges can push C01 below zero because the model is only a curve-fitting form. It is acceptable as long as the shear modulus 2(C10 + C01) stays positive.
When should I use Mooney-Rivlin instead of neo-Hookean?+
Use it when the neo-Hookean curve misses the initial softening or the upturn of your uniaxial data, or when you must also fit shear or biaxial data. Neo-Hookean is usually adequate only below roughly 20 to 40 percent strain.
What are the limits of the Mooney-Rivlin model?+
It has no finite chain extensibility, so it does not capture the sharp stiffening near the chain limit, and fitted constants from one deformation mode may poorly predict another. Models such as Ogden or Arruda-Boyce cover these cases.

📚 Sources and Notes

The form of the strain energy, the history of the model and the neo-Hookean special case follow the Wikipedia article on the Mooney-Rivlin solid and the neo-Hookean solid article. The entropic basis of rubber elasticity is described in the Wikipedia article on rubber elasticity. The uniaxial and equibiaxial stress expressions follow from the incompressible Cauchy stress σi = −p + 2 C10 λi2 − 2 C01 λi−2. The default constants and data points are illustrative, constructed for the examples, and not measurements of a real material.

See also the polymer physics calculators and the true strain calculator.

What is the Mooney-Rivlin model?

The Mooney-Rivlin model is a two-parameter hyperelastic law for rubber with strain energy W = C10 (I1 - 3) + C01 (I2 - 3). It reduces to the neo-Hookean model when C01 = 0 and often fits uniaxial rubber data over a wider stretch range.

What is the uniaxial stress formula for a Mooney-Rivlin solid?

The engineering stress is s = 2 (lambda - lambda^-2)(C10 + C01 / lambda). With C10 = 0.25 MPa, C01 = 0.10 MPa and lambda = 2, s = 2 x 1.75 x 0.30 = 1.050 MPa, and the true stress is s x lambda = 2.100 MPa.

How do you find the shear modulus from C10 and C01?

The initial shear modulus is mu = 2 (C10 + C01). For C10 = 0.25 MPa and C01 = 0.10 MPa, mu = 0.70 MPa. The small-strain Young modulus of an incompressible rubber is about 3 mu, which is 2.1 MPa.

What is a Mooney plot?

A Mooney plot graphs the reduced stress s* = s / (2 (lambda - lambda^-2)) against 1/lambda. For a Mooney-Rivlin solid this is a straight line with intercept C10 and slope C01. A horizontal line means neo-Hookean behavior.

How do you fit C10 and C01 from two data points?

Compute the reduced stress at each stretch, then C01 = (s1* - s2*) / (1/lambda1 - 1/lambda2) and C10 = s1* - C01 / lambda1. For (1.5, 0.6685) and (3.0, 1.637) MPa this gives C10 = 0.2500 and C01 = 0.1000 MPa.

What is the neo-Hookean limit?

Setting C01 = 0 gives the neo-Hookean model with mu = 2 C10, in which the Mooney plot is flat. The stress becomes s = 2 C10 (lambda - lambda^-2), so one constant describes the response.

What is the equibiaxial stress in the Mooney-Rivlin model?

The engineering stress under equibiaxial stretch is s = 2 (lambda - lambda^-5)(C10 + C01 lambda^2). With C10 = 0.25, C01 = 0.10 MPa and lambda = 2 this is 2.559 MPa, noticeably higher than the uniaxial value because the C01 term grows with lambda squared.

Why is C01 sometimes negative?

Fits to wide stretch ranges can push C01 below zero because the model is only a curve-fitting form. It is acceptable as long as the shear modulus 2(C10 + C01) stays positive.

When should I use Mooney-Rivlin instead of neo-Hookean?

Use it when the neo-Hookean curve misses the initial softening or the upturn of your uniaxial data, or when you must also fit shear or biaxial data. Neo-Hookean is usually adequate only below roughly 20 to 40 percent strain.

What are the limits of the Mooney-Rivlin model?

It has no finite chain extensibility, so it does not capture the sharp stiffening near the chain limit, and fitted constants from one deformation mode may poorly predict another. Models such as Ogden or Arruda-Boyce cover these cases.