Vickers Hardness Number Calculator
Turn the diagonal of a diamond pyramid indent into a Vickers number, or work out the indent for a given hardness and load.
💎 What is the Vickers Hardness Number?
The Vickers hardness number (HV, also called the diamond pyramid hardness) measures how well a material resists being dented by a hard point. A diamond in the shape of a square pyramid, with 136 degrees between opposite faces, is pressed into a polished surface under a known load, held for a set time, and removed. The indent left behind is a small square. Its two diagonals are measured under a microscope, and the hardness is the load divided by the surface area of the indent. Harder material resists the point, so the diagonal is shorter and the number is higher. The method was introduced at Vickers Ltd in 1921 as an alternative to the Brinell test.
The strength of the Vickers test is that one indenter and one formula work for almost everything, from soft aluminium and lead to hardened tool steel and ceramics. The indent keeps the same geometric shape at any load, so values from different loads are broadly comparable. Typical loads run from 1 kgf to 100 kgf in the macro range, and lighter loads below 1 kgf are used for microhardness work on thin coatings, single grains, wires and case-hardened layers. A hardness is quoted with its load, for example 350 HV30, because results can drift with load on some materials. The number is quoted without units, although it is a force per area, kgf per square millimetre.
Typical uses include checking heat treatment on steel parts, measuring the depth profile of a carburised or nitrided case, testing welds and heat-affected zones across a fusion line, and comparing small or thin parts that a ball or a Rockwell cone would damage. The accuracy depends on a flat polished surface, a stable load, careful focus and a mean of both diagonals. The specimen must be thick enough, at least 1.5 times the diagonal, that the support does not affect the result, and indents must be spaced far enough apart. The estimate of tensile strength shown here is a rough rule for steels only.
This page works from the load and the measured diagonal. For a comparison with other methods see the Brinell hardness calculator, and for approximate conversion between scales use the Rockwell hardness conversion calculator. Strength itself is in the tensile strength calculator, and toughness is a different property again, covered by the impact test calculator.
📐 Formula
📖 How to Use This Calculator
Steps
💡 Example Calculations
Example 1 — An HV30 Test on a Steel Part
A 30 kgf load leaves an indent with a mean diagonal of 0.4 mm
Example 2 — A Light Load Entered in Newtons
A 9.80665 N load (exactly 1 kgf) leaves a 0.05 mm diagonal on a thin hard layer
Example 3 — Expected Indent for 350 HV
A material of 350 HV is to be tested at 30 kgf. How big will the indent be?
Example 4 — A Hardened Tool Steel
A tool steel of 800 HV is tested at 10 kgf
Example 5 — Choosing a Load for 350 HV
Compare the expected indents of a 350 HV material across the common loads
❓ Frequently Asked Questions
🔗 Related Calculators
How do you calculate the Vickers hardness number?
HV = 1.8544 F / d squared, with F the load in kgf and d the mean diagonal in mm. A 30 kgf load with a 0.4 mm diagonal gives 347.7 HV, written 347.7 HV30.
Where does the 1.8544 come from?
The indenter is a square pyramid with 136 degrees between opposite faces. The surface area of the indent is d squared divided by 2 sin(68 degrees), so HV = F / area = 2 sin(68 degrees) F / d squared, which is 1.8544 F / d squared.
How do I use newtons instead of kgf?
Divide the force in newtons by 9.80665 to get kgf, or use HV = 0.1891 F / d squared with F in newtons. Choose N in the unit box and the calculator does it. 294.2 N is 30 kgf.
What do HV1 to HV100 mean?
The number after HV is the test load in kgf, so HV10 uses 10 kgf and HV30 uses 30 kgf. Loads below 1 kgf are called microhardness tests, and the same formula applies.
How deep is a Vickers indent?
About one seventh of the mean diagonal, d / 7. A 0.4 mm diagonal means a depth near 57 micrometres, which is why the test needs a specimen at least 1.5 times the diagonal thick.
How do you convert Vickers hardness to tensile strength?
For steels a rough rule is about 3.2 MPa per HV, so 350 HV is near 1120 MPa. It is only an estimate, and it does not hold for most other metals or for very hard or soft steels.
Does the Vickers number have units?
Strictly it is a force per area, kgf per square millimetre, but it is quoted without units. Multiplying by 9.80665 and dividing by 1000 gives the same figure as a mean contact pressure in GPa.
How is Vickers different from Brinell and Rockwell?
Vickers uses a diamond pyramid and one formula for all hardnesses, so it covers soft metals to hard ceramics. Brinell uses a ball and suits coarse structures, and Rockwell reads depth directly for fast production testing.
Why should I choose the load carefully?
A light load gives a tiny indent that is hard to measure and sensitive to surface finish, and a heavy load averages over more material but needs a thicker specimen. Pick a load that gives a diagonal you can read comfortably.
What is the Vickers hardness of steel?
Mild steel is around 120 to 200 HV, hardened tool steel can be 700 HV or more. These are indicative figures. Quote tested values with their load.
Can I convert HV to Rockwell or Brinell?
Only approximately, with a table for each material class. See the Rockwell conversion and the Brinell hardness pages. Conversions are not exact and should not be used for certification.