Rockwell Hardness Conversion Calculator
Estimate the Vickers, Brinell and strength equivalents of a Rockwell C reading on steel, and see how the A, B and C scales are built.
🔧 What is Rockwell Hardness Conversion?
The Rockwell hardness test measures how deep an indenter sinks into a material under a fixed load. A small minor load seats the indenter and sets a zero, a larger major load is added, and then the major load is removed. The permanent increase in depth, in units of 0.002 mm, becomes the Rockwell number, so a harder material, which is dented less, gets a higher number. Because it reads depth directly with no microscope, the test is fast and is the workhorse of production heat-treatment checks. Results carry a letter for the scale, such as HRC, HRB or HRA, since each scale uses a different indenter and load.
Hardness conversion is the practice of estimating the reading on one scale from a reading on another, for example from HRC to Vickers (HV) or Brinell (HBW). People do it because a drawing may call for one scale while the shop has a different tester, or because a report quotes a scale they do not use. It is also done to estimate tensile strength, because for steels hardness and strength rise together in a roughly linear way. The important point is that every such conversion is an approximation. The scales respond to different things, and the relationship was measured on specific materials, mostly non-austenitic steels.
That is why this page is written with care. It holds a small illustrative table of rounded values for steel at HRC 20, 25 and so on up to 65, and interpolates linearly between rows. It is meant for a rough sense of scale, not for certification or acceptance. The full standards, ASTM E140 and ISO 18265, publish complete tables, each tied to a material class, and they state that the best practice is to test directly in the required scale. Stainless steels, cast iron, copper alloys and aluminium need their own tables, and hardened or nitrided surface layers can differ from the core. The scales mode of the calculator also explains how the A, B and C scales are built, with the indenter, the minor and major loads and the usual range.
To work out hardness from an indent rather than convert it, use the Vickers hardness calculator or the Brinell hardness calculator. For strength see the tensile strength calculator and the stress-strain calculator, and for toughness see the impact test calculator.
📐 Formula
📖 How to Use This Calculator
Steps
💡 Example Calculations
Example 1 — A Table Row, HRC 45
A quenched and tempered steel reads 45 HRC
Example 2 — Between Rows, HRC 42
A part reads 42 HRC, between the 40 and 45 rows
Example 3 — Very Hard Steel, HRC 58
A tool steel reads 58 HRC
Example 4 — From Vickers Back to Rockwell C
A report gives 500 HV and the shop only has a Rockwell C tester
Example 5 — From Brinell Back to Rockwell C
A casting certificate gives 300 HBW
Example 6 — Reading the C Scale From Depth
The permanent depth increase on scale C is 0.1 mm
Example 7 — The Same Depth on the B Scale
The permanent depth increase on scale B is 0.1 mm
❓ Frequently Asked Questions
🔗 Related Calculators
How do you convert HRC to HV?
There is no exact formula. Conversion uses a table of paired readings measured on steel and interpolates between rows. In the table used here HRC 40 is about 392 HV and HRC 50 is about 513 HV. The values are approximate.
What is HRC 45 in Brinell?
About 421 HBW in the illustrative steel table used here, with roughly 446 HV and a tensile strength near 1450 MPa. Treat these as rough equivalents, not certified values.
Are hardness conversions accurate?
Only roughly. Each scale measures a different response, so conversion is a statistical correlation for one material class. Standards such as ASTM E140 say conversions are approximate and that the best practice is to test in the required scale.
What is the difference between HRA, HRB and HRC?
They use different indenters and loads. HRC uses a diamond cone and 150 kgf for hardened steel, HRB uses a 1/16 inch steel ball and 100 kgf for softer metals, and HRA uses a diamond cone and 60 kgf for thin or very hard material.
What are the minor and major loads?
The tester first applies a minor load of 10 kgf to seat the indenter and set a zero, then adds the major load, then returns to the minor load. The permanent depth difference gives the Rockwell number.
How is the Rockwell number calculated?
As HR = N minus h divided by 0.002 mm, with h the permanent depth increase and N equal to 100 for the diamond scales and 130 for the ball scales. A depth of 0.1 mm on scale C gives 50 HRC.
Why is there no Brinell value above about HRC 50?
A tungsten carbide ball deforms on very hard steel, so the Brinell test becomes unreliable and tables stop listing values. Use Vickers or Rockwell for hard steel.
Can I convert aluminium or stainless steel with this table?
No. The table is for non-austenitic steels. Other alloys follow different relationships, and published tables exist for each class.
What is the valid range of the HRC scale?
Usually about 20 to 70 HRC. Below 20 the result is unreliable and a softer scale such as HRB is used. The table here covers 20 to 65.
How is this related to the Vickers and Brinell calculators?
They calculate hardness from an indent: the Vickers page from the diagonal of a diamond pyramid and the Brinell page from the diameter of a ball impression. This page only converts between scales roughly.
Can I use these values for certification?
No. The table is small and illustrative and the conversion is approximate. For compliance, test in the scale the specification requires with a calibrated machine.