Rockwell Hardness Conversion Calculator

Estimate the Vickers, Brinell and strength equivalents of a Rockwell C reading on steel, and see how the A, B and C scales are built.

🔧 Rockwell Hardness Conversion Calculator
Rockwell C hardness20 to 65, steel
HRC
Scale you have
Hardness value
HV / HBW
Rockwell scale
Permanent depth increase heach Rockwell point is 0.002 mm
mm
Approximate Vickers hardness
—
Approximate Brinell hardness
—
Approximate tensile strength
—
Mean contact pressure
—
Range check
—
Scale used
—

Approximate Rockwell C
—
Vickers hardness
—
Brinell hardness
—
Approximate tensile strength
—
Input
—

Rockwell number
—
Indenter
—
Minor load
—
Major (total) load
—
Usual range of the scale
—
Validity check
—
Typical use
—

🔧 What is Rockwell Hardness Conversion?

The Rockwell hardness test measures how deep an indenter sinks into a material under a fixed load. A small minor load seats the indenter and sets a zero, a larger major load is added, and then the major load is removed. The permanent increase in depth, in units of 0.002 mm, becomes the Rockwell number, so a harder material, which is dented less, gets a higher number. Because it reads depth directly with no microscope, the test is fast and is the workhorse of production heat-treatment checks. Results carry a letter for the scale, such as HRC, HRB or HRA, since each scale uses a different indenter and load.

Hardness conversion is the practice of estimating the reading on one scale from a reading on another, for example from HRC to Vickers (HV) or Brinell (HBW). People do it because a drawing may call for one scale while the shop has a different tester, or because a report quotes a scale they do not use. It is also done to estimate tensile strength, because for steels hardness and strength rise together in a roughly linear way. The important point is that every such conversion is an approximation. The scales respond to different things, and the relationship was measured on specific materials, mostly non-austenitic steels.

That is why this page is written with care. It holds a small illustrative table of rounded values for steel at HRC 20, 25 and so on up to 65, and interpolates linearly between rows. It is meant for a rough sense of scale, not for certification or acceptance. The full standards, ASTM E140 and ISO 18265, publish complete tables, each tied to a material class, and they state that the best practice is to test directly in the required scale. Stainless steels, cast iron, copper alloys and aluminium need their own tables, and hardened or nitrided surface layers can differ from the core. The scales mode of the calculator also explains how the A, B and C scales are built, with the indenter, the minor and major loads and the usual range.

To work out hardness from an indent rather than convert it, use the Vickers hardness calculator or the Brinell hardness calculator. For strength see the tensile strength calculator and the stress-strain calculator, and for toughness see the impact test calculator.

📐 Formula

HR = N − h ÷ 0.002 mm    (conversion: linear interpolation in a table)
HR = the Rockwell number on the chosen scale. h = the permanent increase in depth in mm, after returning to the minor load.
N = 100 for the diamond cone scales (A and C) and 130 for the ball scales (B). Each Rockwell point is 0.002 mm of depth.
Scale C: diamond cone, minor load 10 kgf, major load 150 kgf, usual range about 20 to 70. Scale B: 1/16 in steel ball, 10 kgf and 100 kgf, usual range about 20 to 100. Scale A: diamond cone, 10 kgf and 60 kgf, usual range about 20 to 88.
Conversion (approximate): a value between two table rows is found by y = y1 + (HRC − HRC1) / (HRC2 − HRC1) × (y2 − y1), with the table rounded and illustrative, for non-austenitic steels only.
Example: a depth of 0.1 mm on scale C gives HRC = 100 − 0.1 / 0.002 = 50. HRC 45 converts to about 446 HV, 421 HBW and 1450 MPa.

📖 How to Use This Calculator

Steps

1
Choose a mode. Use HRC to other scales for a forward conversion, HV or HBW to HRC for the reverse, or Scales and loads for the A, B and C details.
2
Enter the reading. Type the HRC number, or the Vickers or Brinell value, or the scale and the permanent depth in mm.
3
Read the approximate result. The results show the approximate equivalents, the range check and a chart or table. Treat every converted value as approximate and not for certification.

💡 Example Calculations

Example 1 — A Table Row, HRC 45

A quenched and tempered steel reads 45 HRC

1
HRC 45 is a row of the illustrative table, so no interpolation is needed.
2
The row gives about 446 HV and 421 HBW.
3
The rough tensile strength is 1450 MPa (210 ksi), and the mean contact pressure is 446 × 9.80665 / 1000 = 4.37 GPa.
HRC 45 ≈ 446 HV, 421 HBW, 1450 MPa (approximate)
Try this example →

Example 2 — Between Rows, HRC 42

A part reads 42 HRC, between the 40 and 45 rows

1
The fraction is (42 − 40) / (45 − 40) = 0.4.
2
HV = 392 + 0.4 × (446 − 392) = 414 (413.6). HBW = 371 + 0.4 × 50 = 391.
3
Strength = 1250 + 0.4 × 200 = 1330 MPa (193 ksi).
HRC 42 ≈ 414 HV, 391 HBW, 1330 MPa (approximate)
Try this example →

Example 3 — Very Hard Steel, HRC 58

A tool steel reads 58 HRC

1
The fraction between the 55 and 60 rows is (58 − 55) / 5 = 0.6.
2
HV = 595 + 0.6 × (697 − 595) = 656 (656.2).
3
The table gives no Brinell value in this range, because a carbide ball is unreliable on steel this hard, and no strength estimate, because the correlation is not trusted.
HRC 58 ≈ 656 HV, no HBW or strength given
Try this example →

Example 4 — From Vickers Back to Rockwell C

A report gives 500 HV and the shop only has a Rockwell C tester

1
500 HV sits between the 45 HRC row (446 HV) and the 50 HRC row (513 HV).
2
HRC = 45 + 5 × (500 − 446) / (513 − 446) = 49.0 (49.03).
3
At that HRC the table gives about 469 HBW and 1660 MPa (241 ksi).
500 HV ≈ 49.0 HRC, 469 HBW (approximate)
Try this example →

Example 5 — From Brinell Back to Rockwell C

A casting certificate gives 300 HBW

1
300 HBW sits between the 30 HRC row (286 HBW) and the 35 HRC row (327 HBW).
2
HRC = 30 + 5 × (300 − 286) / (327 − 286) = 31.7.
3
The other columns give about 317 HV and 994 MPa (144 ksi).
300 HBW ≈ 31.7 HRC, 317 HV (approximate)
Try this example →

Example 6 — Reading the C Scale From Depth

The permanent depth increase on scale C is 0.1 mm

1
h / 0.002 = 0.1 / 0.002 = 50 points of depth.
2
HRC = 100 − 50 = 50.0 HRC.
3
The loads are a 10 kgf minor load (98.1 N) and a 150 kgf major load (1471 N), and 50 is inside the usual 20 to 70 range.
Depth 0.1 mm on scale C = 50.0 HRC
Try this example →

Example 7 — The Same Depth on the B Scale

The permanent depth increase on scale B is 0.1 mm

1
The ball scales use N = 130, so HRB = 130 − 0.1 / 0.002 = 130 − 50 = 80.0 HRB.
2
The indenter is a 1/16 in steel ball and the major load is 100 kgf (981 N).
3
80 lies inside the usual HRB range of 20 to 100, so B is a sensible scale for this softer steel or brass.
Depth 0.1 mm on scale B = 80.0 HRB
Try this example →

❓ Frequently Asked Questions

How do you convert HRC to HV?+
There is no exact formula. Conversion uses a table of paired readings measured on steel and interpolates between rows. In the table used here HRC 40 is about 392 HV and HRC 50 is about 513 HV. The values are approximate.
What is HRC 45 in Brinell?+
About 421 HBW in the illustrative steel table used here, with roughly 446 HV and a tensile strength near 1450 MPa. Treat these as rough equivalents, not certified values.
Are hardness conversions accurate?+
Only roughly. Each scale measures a different response, so conversion is a statistical correlation for one material class. Standards such as ASTM E140 say conversions are approximate and that the best practice is to test in the required scale.
What is the difference between HRA, HRB and HRC?+
They use different indenters and loads. HRC uses a diamond cone and 150 kgf for hardened steel, HRB uses a 1/16 inch steel ball and 100 kgf for softer metals, and HRA uses a diamond cone and 60 kgf for thin or very hard material.
What are the minor and major loads?+
The tester first applies a minor load of 10 kgf to seat the indenter and set a zero, then adds the major load, then returns to the minor load. The permanent depth difference gives the Rockwell number.
How is the Rockwell number calculated?+
As HR = N minus h divided by 0.002 mm, with h the permanent depth increase and N equal to 100 for the diamond scales and 130 for the ball scales. A depth of 0.1 mm on scale C gives 50 HRC.
Why is there no Brinell value above about HRC 50?+
A tungsten carbide ball deforms on very hard steel, so the Brinell test becomes unreliable and tables stop listing values. Use Vickers or Rockwell for hard steel.
Can I convert aluminium or stainless steel with this table?+
No. The table is for non-austenitic steels. Other alloys follow different relationships, and published tables exist for each class.
What is the valid range of the HRC scale?+
Usually about 20 to 70 HRC. Below 20 the result is unreliable and a softer scale such as HRB is used. The table here covers 20 to 65.
How is this related to the Vickers and Brinell calculators?+
They calculate hardness from an indent: the Vickers page from the diagonal of a diamond pyramid and the Brinell page from the diameter of a ball impression. This page only converts between scales roughly.
Can I use these values for certification?+
No. The table is small and illustrative and the conversion is approximate. For compliance, test in the scale the specification requires with a calibrated machine.

How do you convert HRC to HV?

There is no exact formula. Conversion uses a table of paired readings measured on steel and interpolates between rows. In the table used here HRC 40 is about 392 HV and HRC 50 is about 513 HV. The values are approximate.

What is HRC 45 in Brinell?

About 421 HBW in the illustrative steel table used here, with roughly 446 HV and a tensile strength near 1450 MPa. Treat these as rough equivalents, not certified values.

Are hardness conversions accurate?

Only roughly. Each scale measures a different response, so conversion is a statistical correlation for one material class. Standards such as ASTM E140 say conversions are approximate and that the best practice is to test in the required scale.

What is the difference between HRA, HRB and HRC?

They use different indenters and loads. HRC uses a diamond cone and 150 kgf for hardened steel, HRB uses a 1/16 inch steel ball and 100 kgf for softer metals, and HRA uses a diamond cone and 60 kgf for thin or very hard material.

What are the minor and major loads?

The tester first applies a minor load of 10 kgf to seat the indenter and set a zero, then adds the major load, then returns to the minor load. The permanent depth difference gives the Rockwell number.

How is the Rockwell number calculated?

As HR = N minus h divided by 0.002 mm, with h the permanent depth increase and N equal to 100 for the diamond scales and 130 for the ball scales. A depth of 0.1 mm on scale C gives 50 HRC.

Why is there no Brinell value above about HRC 50?

A tungsten carbide ball deforms on very hard steel, so the Brinell test becomes unreliable and tables stop listing values. Use Vickers or Rockwell for hard steel.

Can I convert aluminium or stainless steel with this table?

No. The table is for non-austenitic steels. Other alloys follow different relationships, and published tables exist for each class.

What is the valid range of the HRC scale?

Usually about 20 to 70 HRC. Below 20 the result is unreliable and a softer scale such as HRB is used. The table here covers 20 to 65.

How is this related to the Vickers and Brinell calculators?

They calculate hardness from an indent: the Vickers page from the diagonal of a diamond pyramid and the Brinell page from the diameter of a ball impression. This page only converts between scales roughly.

Can I use these values for certification?

No. The table is small and illustrative and the conversion is approximate. For compliance, test in the scale the specification requires with a calibrated machine.