Brinell Hardness Number Calculator

Turn the indent left by a hardened ball into a Brinell number, or work out the indent and the test load for a given hardness.

🔘 Brinell Hardness Number Calculator
Standard test (optional)fills the ball and force
Ball diameter D
Test force F
Mean indent diameter d
mm
Brinell hardness
HBW
Load ratio 0.102 F / D²kgf per mm²
Brinell hardness
—
Test designation
—
Test force
—
Load ratio
—
Indent depth
—
Validity check
—
Tensile strength, rough estimate (steels)
—
Mean contact pressure
—

Indent diameter d
—
Test designation
—
Test force
—
Load ratio
—
Indent depth
—
Validity check
—
Tensile strength, rough estimate (steels)
—

Test force
—
Test force in newtons
—
Test designation
—
Lowest valid hardness (d = 0.6 D)
—
Highest valid hardness (d = 0.24 D)
—
Typical use of this ratio
—
Load ratio
—
Indent depth range
—

🔘 What is the Brinell Hardness Number?

The Brinell hardness number, written HBW when a tungsten carbide ball is used, measures how well a metal resists being indented. A hard ball, usually 10 mm across, is pressed into the surface under a fixed force, typically 3000 kgf for steel, and held for a set time. After the force is removed the diameter of the circular dent is measured with a microscope, and the hardness is the force divided by the curved surface area of the dent. A smaller dent under the same force means a harder material, so a higher number.

The test is widely used for castings, forgings and bar stock in foundries, steel mills and quality labs. Its large ball and large indent average over the grain structure, which suits coarse or non-uniform materials such as cast iron where a small indent would wander. Typical uses are acceptance testing of heat-treated parts, checking that a supplied bar meets its specified hardness range, and quickly screening a batch without cutting a tensile specimen. A hardness reading is also easy to take on a finished part, which a tensile test is not.

The figure is reported with the test conditions, such as HBW 10/3000, meaning a 10 mm ball under 3000 kgf. Standards limit the indent diameter to between 0.24 and 0.6 of the ball diameter, because outside that window the result stops being comparable. They also recommend holding the load ratio, 0.102 F divided by D squared, constant, so that indents made with different balls have the same shape. This calculator gives the number from the force, ball and indent, the indent you should expect from a known hardness, and the load that matches a chosen ratio and ball.

Hardness is not strength. Many steels show a rough proportion between hardness and ultimate tensile strength, so you will see rules of thumb such as tensile strength in MPa of about 3.45 times HBW. This page shows that figure, but flags it as a rough estimate for carbon and low-alloy steels only. It differs from the tensile strength calculator, which finds stress from a force and a cross-section, and from the stress-strain calculator, which measures stiffness. For conversions between kg and newtons see the kg to newtons calculator.

📐 Formula

HBW = 2F / (π D (D − √(D2 − d2)))
F = test force in kgf. If the force is in newtons, divide by 9.80665 first; the ISO form multiplies by 0.102, which is 1 / 9.80665 rounded.
D = ball diameter in mm (commonly 10, 5, 2.5, 2 or 1 mm) and d = mean indent diameter in mm.
Load ratio: 0.102 F / D2, equal to F in kgf divided by D2. Standard ratios are 30, 15, 10, 5, 2.5, 1.25 and 1. For example 30 × 102 = 3000 kgf.
Indent depth: h = D − √(D2 − d2) = 2F / (π D HBW), so d = √(2 D h − h2).
Valid window: 0.24 D ≤ d ≤ 0.6 D. For a ratio of 30 that is about 95.5 to 653.5 HBW.
Rough tensile estimate (steels only): UTS ≈ 3.45 × HBW in MPa, for roughly 100 to 400 HBW. Treat it as an estimate, not a property.
Example: F = 3000 kgf, D = 10 mm, d = 4.0 mm give HBW = 6000 / (π × 10 × 0.83485) = 228.8.

📖 How to Use This Calculator

Steps

1
Set the test. Pick a standard test preset or choose the ball diameter and enter the force, selecting kgf or N. The unit box only changes how your number is read.
2
Choose a mode. Use Hardness from indent to turn a measured dent into HBW, Indent from hardness to predict the dent, or Test load to pick a ball and load ratio.
3
Enter the reading. Type the mean indent diameter in mm or the Brinell hardness, or select the load ratio in the planner.
4
Check the results. Read the hardness, the designation, the load ratio and the d / D validity check. The tensile estimate is rough and only for steels.

💡 Example Calculations

Example 1 — A Standard Steel Test

A 10 mm ball under 3000 kgf leaves an indent 4.0 mm across

1
√(102 − 42) = √84 = 9.16515, so D − √(D2 − d2) = 0.83485 mm.
2
HBW = 2 × 3000 / (π × 10 × 0.83485) = 6000 / 26.227 = 228.8.
3
The load ratio is 30 (standard) and d / D = 0.400 is inside the valid window. The rough steel estimate is 3.45 × 228.8 = 789 MPa.
Hardness = 228.8 HBW, designation HBW 10/3000
Try this example →

Example 2 — A Force Given in Newtons

A test frame reports 29,420 N on a 10 mm ball and the indent measures 4.5 mm

1
F = 29,420 / 9.80665 = 3000 kgf, so this is a HBW 10/3000 test.
2
√(100 − 20.25) = 8.93028, so the depth is 1.0697 mm.
3
HBW = 6000 / (π × 10 × 1.0697) = 178.5, and the rough steel estimate is 616 MPa.
Hardness = 178.5 HBW
Try this example →

Example 3 — Predicting the Indent

A bar of 180 HBW is tested with a 10 mm ball under 3000 kgf

1
Depth h = 2 × 3000 / (π × 10 × 180) = 1.0610 mm.
2
d = √(2 × 10 × 1.0610 − 1.06102) = √20.095 = 4.483 mm.
3
d / D = 0.448 is within 0.24 to 0.60, so the test is valid.
Expected indent diameter = 4.483 mm
Try this example →

Example 4 — Choosing a Load for a 5 mm Ball

A 5 mm ball with a load ratio of 10, as used for copper and aluminium alloys (illustrative)

1
F = 10 × 52 = 250 kgf = 250 × 9.80665 = 2,451.7 N.
2
The designation is HBW 5/250.
3
At d = 0.6 D the hardness is 31.8 HBW, and at d = 0.24 D it is 217.8 HBW, so the test covers that range.
Test = HBW 5/250, valid from 31.8 to 217.8 HBW
Try this example →

Example 5 — A Soft Metal

A 10 mm ball under 500 kgf leaves a 3.2 mm indent in a soft alloy

1
√(100 − 10.24) = 9.47417, so the depth is 0.5258 mm.
2
HBW = 1000 / (π × 10 × 0.5258) = 60.5, with a load ratio of 5.
3
60.5 is below 100 HBW, so the steel tensile rule does not apply and the calculator says so.
Hardness = 60.5 HBW, designation HBW 10/500
Try this example →

❓ Frequently Asked Questions

How do you calculate the Brinell hardness number?+
HBW = 2F / (pi D (D minus the square root of D squared minus d squared)), with F in kgf, D the ball diameter in mm and d the mean indent diameter in mm. A 3000 kgf load, a 10 mm ball and a 4.0 mm indent give 228.8 HBW.
What do HBW 10/3000 and similar codes mean?+
The first number is the ball diameter in mm and the second is the test force in kgf. HBW 10/3000 is a 10 mm tungsten carbide ball under 3000 kgf, the usual test for steel.
What is the load ratio in Brinell testing?+
It is 0.102 F / D squared with F in newtons, which equals F in kgf divided by D squared. Standard ratios include 30, 10, 5, 2.5 and 1. A ratio of 30 with a 10 mm ball gives 3000 kgf.
Can I enter the force in newtons?+
Yes. Choose N in the unit box. The calculator divides by 9.80665 to get kgf, so 29420 N is 3000 kgf and gives the same hardness.
What is the valid range of indent diameter?+
The indent diameter should be between 0.24 and 0.6 of the ball diameter. For a 10 mm ball under 3000 kgf that corresponds to roughly 95 to 654 HBW.
How do you convert Brinell hardness to tensile strength?+
For carbon and low-alloy steels from about 100 to 400 HBW a common rough estimate is tensile strength in MPa of about 3.45 times HBW. 228.8 HBW gives about 789 MPa. It is only an estimate and can be off by a wide margin.
Does the Brinell number have units?+
Strictly it is a force per area, kgf per square millimetre, but it is quoted without units. Multiplying by 9.80665 gives the same figure as a mean contact pressure in MPa.
What does HBW mean compared with HB or HBS?+
HBW means the test used a tungsten carbide ball. Older reports use HB or HBS, with HBS for a hardened steel ball. The formula is the same.
Why would I find the indent diameter from a hardness?+
It tells you what indent to expect before testing, and whether it will fall inside the valid window. A material of 180 HBW under 3000 kgf with a 10 mm ball should leave an indent about 4.483 mm across.
How is this different from a tensile strength calculator?+
A tensile strength calculator finds stress from force and area. Brinell hardness measures resistance to indentation, and the tensile figure here is only a rough correlation from it.
Which ball and load should I choose?+
Use a 10 mm ball at ratio 30 (3000 kgf) for steels and cast irons, and lighter ratios such as 10 or 5 for softer alloys. Choose the test so that the indent falls between 0.24 D and 0.6 D, and use the Test load mode to check the valid hardness window.

How do you calculate the Brinell hardness number?

HBW = 2F / (pi D (D minus the square root of D squared minus d squared)), with F in kgf, D the ball diameter in mm and d the mean indent diameter in mm. A 3000 kgf load, a 10 mm ball and a 4.0 mm indent give 228.8 HBW.

What do HBW 10/3000 and similar codes mean?

The first number is the ball diameter in mm and the second is the test force in kgf. HBW 10/3000 is a 10 mm tungsten carbide ball under 3000 kgf, the usual test for steel.

What is the load ratio in Brinell testing?

It is 0.102 F / D squared with F in newtons, which equals F in kgf divided by D squared. Standard ratios include 30, 10, 5, 2.5 and 1. A ratio of 30 with a 10 mm ball gives 3000 kgf.

Can I enter the force in newtons?

Yes. Choose N in the unit box. The calculator divides by 9.80665 to get kgf, so 29420 N is 3000 kgf and gives the same hardness.

What is the valid range of indent diameter?

The indent diameter should be between 0.24 and 0.6 of the ball diameter. For a 10 mm ball under 3000 kgf that corresponds to roughly 95 to 654 HBW.

How do you convert Brinell hardness to tensile strength?

For carbon and low-alloy steels from about 100 to 400 HBW a common rough estimate is tensile strength in MPa of about 3.45 times HBW. 228.8 HBW gives about 789 MPa. It is only an estimate and can be off by a wide margin.

Does the Brinell number have units?

Strictly it is a force per area, kgf per square millimetre, but it is quoted without units. Multiplying by 9.80665 gives the same figure as a mean contact pressure in MPa.

What does HBW mean compared with HB or HBS?

HBW means the test used a tungsten carbide ball. Older reports use HB or HBS, with HBS for a hardened steel ball. The formula is the same.

Why would I find the indent diameter from a hardness?

It tells you what indent to expect before testing, and whether it will fall inside the valid window. A material of 180 HBW under 3000 kgf with a 10 mm ball should leave an indent about 4.483 mm across.

How is this different from a tensile strength calculator?

A tensile strength calculator finds stress from force and area. Brinell hardness measures resistance to indentation, and the tensile figure here is only a rough correlation from it.