Brinell Hardness Number Calculator
Turn the indent left by a hardened ball into a Brinell number, or work out the indent and the test load for a given hardness.
🔘 What is the Brinell Hardness Number?
The Brinell hardness number, written HBW when a tungsten carbide ball is used, measures how well a metal resists being indented. A hard ball, usually 10 mm across, is pressed into the surface under a fixed force, typically 3000 kgf for steel, and held for a set time. After the force is removed the diameter of the circular dent is measured with a microscope, and the hardness is the force divided by the curved surface area of the dent. A smaller dent under the same force means a harder material, so a higher number.
The test is widely used for castings, forgings and bar stock in foundries, steel mills and quality labs. Its large ball and large indent average over the grain structure, which suits coarse or non-uniform materials such as cast iron where a small indent would wander. Typical uses are acceptance testing of heat-treated parts, checking that a supplied bar meets its specified hardness range, and quickly screening a batch without cutting a tensile specimen. A hardness reading is also easy to take on a finished part, which a tensile test is not.
The figure is reported with the test conditions, such as HBW 10/3000, meaning a 10 mm ball under 3000 kgf. Standards limit the indent diameter to between 0.24 and 0.6 of the ball diameter, because outside that window the result stops being comparable. They also recommend holding the load ratio, 0.102 F divided by D squared, constant, so that indents made with different balls have the same shape. This calculator gives the number from the force, ball and indent, the indent you should expect from a known hardness, and the load that matches a chosen ratio and ball.
Hardness is not strength. Many steels show a rough proportion between hardness and ultimate tensile strength, so you will see rules of thumb such as tensile strength in MPa of about 3.45 times HBW. This page shows that figure, but flags it as a rough estimate for carbon and low-alloy steels only. It differs from the tensile strength calculator, which finds stress from a force and a cross-section, and from the stress-strain calculator, which measures stiffness. For conversions between kg and newtons see the kg to newtons calculator.
📐 Formula
📖 How to Use This Calculator
Steps
💡 Example Calculations
Example 1 — A Standard Steel Test
A 10 mm ball under 3000 kgf leaves an indent 4.0 mm across
Example 2 — A Force Given in Newtons
A test frame reports 29,420 N on a 10 mm ball and the indent measures 4.5 mm
Example 3 — Predicting the Indent
A bar of 180 HBW is tested with a 10 mm ball under 3000 kgf
Example 4 — Choosing a Load for a 5 mm Ball
A 5 mm ball with a load ratio of 10, as used for copper and aluminium alloys (illustrative)
Example 5 — A Soft Metal
A 10 mm ball under 500 kgf leaves a 3.2 mm indent in a soft alloy
❓ Frequently Asked Questions
🔗 Related Calculators
How do you calculate the Brinell hardness number?
HBW = 2F / (pi D (D minus the square root of D squared minus d squared)), with F in kgf, D the ball diameter in mm and d the mean indent diameter in mm. A 3000 kgf load, a 10 mm ball and a 4.0 mm indent give 228.8 HBW.
What do HBW 10/3000 and similar codes mean?
The first number is the ball diameter in mm and the second is the test force in kgf. HBW 10/3000 is a 10 mm tungsten carbide ball under 3000 kgf, the usual test for steel.
What is the load ratio in Brinell testing?
It is 0.102 F / D squared with F in newtons, which equals F in kgf divided by D squared. Standard ratios include 30, 10, 5, 2.5 and 1. A ratio of 30 with a 10 mm ball gives 3000 kgf.
Can I enter the force in newtons?
Yes. Choose N in the unit box. The calculator divides by 9.80665 to get kgf, so 29420 N is 3000 kgf and gives the same hardness.
What is the valid range of indent diameter?
The indent diameter should be between 0.24 and 0.6 of the ball diameter. For a 10 mm ball under 3000 kgf that corresponds to roughly 95 to 654 HBW.
How do you convert Brinell hardness to tensile strength?
For carbon and low-alloy steels from about 100 to 400 HBW a common rough estimate is tensile strength in MPa of about 3.45 times HBW. 228.8 HBW gives about 789 MPa. It is only an estimate and can be off by a wide margin.
Does the Brinell number have units?
Strictly it is a force per area, kgf per square millimetre, but it is quoted without units. Multiplying by 9.80665 gives the same figure as a mean contact pressure in MPa.
What does HBW mean compared with HB or HBS?
HBW means the test used a tungsten carbide ball. Older reports use HB or HBS, with HBS for a hardened steel ball. The formula is the same.
Why would I find the indent diameter from a hardness?
It tells you what indent to expect before testing, and whether it will fall inside the valid window. A material of 180 HBW under 3000 kgf with a 10 mm ball should leave an indent about 4.483 mm across.
How is this different from a tensile strength calculator?
A tensile strength calculator finds stress from force and area. Brinell hardness measures resistance to indentation, and the tensile figure here is only a rough correlation from it.